Mass Finishing Sample Trial Record for Small Precision Parts July 20 , 2026

Printable Process-Control Resource

Mass Finishing Sample Trial Record for Small Precision Parts

Use this non-promotional worksheet to define the incoming part, record one controlled finishing trial, compare results, and decide whether the process is ready for a repeat run.

Before sending parts for a trial

Complete Section A below before requesting a process recommendation; there is no need to create a second checklist. Match each sample bag or container to the drawing revision and trial ID, identify any untreated reference parts, and mark the features that must not change. Agree on the inspection locations, method and acceptance limits before processing. If a limit is not yet defined, record it as an open question rather than assuming that a visually brighter part is acceptable.

Before dispatch, confirm sample acceptance and shipping instructions with the team, including which drawings or photographs may be shared, the quantity available for testing, and any handling restrictions. Fees, timing, return arrangements and the scope of testing should be confirmed for the specific request. For equipment context, review the vibratory finishing machine range; a machine selection or production result cannot be established from capacity alone.

How to use this worksheet

  1. Complete the part and acceptance sections before selecting a machine or recipe.
  2. Photograph representative parts under consistent lighting and mark the critical inspection locations.
  3. Run a small representative batch. Change one primary variable at a time.
  4. Inspect at planned intervals instead of extending the cycle by assumption.
  5. Repeat an acceptable trial before releasing a process window for production.

A. Part and acceptance definition

Field Record
Trial ID / date / owner
Part name / drawing revision
Material / hardness / coating
Part size / weight / batch quantity
Incoming defect and location
Critical features to protect Threads / holes / slots / sealing face / sharp edge / cosmetic face / other:
Acceptance criteria Burr limit, edge condition, dimensions, surface appearance, cleanliness and any approved reference sample:
Inspection method Visual standard / magnification / gauge / surface measurement / functional test:

B. Trial recipe and load

Process field Setting or measured value Why selected
Machine / bowl, tub, barrel or magnetic system
Media material / shape / size / condition
Part load / media load / working volume
Compound / water / concentration / flow
Speed / amplitude / direction
Planned inspection times
Separation / rinse / dry method

C. Inspection results by interval

Time Burr / defect Critical edges Dimensions Surface / cleanliness Decision
0 / baseline
Interval 1
Interval 2
Final

D. Failure evidence and next change

Do not record only “pass” or “fail.” Describe where the result appeared, how many inspected parts showed it, and which process variable will be changed next.

Observed pattern Evidence to record Next controlled question
Burr remains Location, direction, size range and affected sample count Is contact missing, media too large, or process energy insufficient?
Edge changes before burr is removed Critical edge measurement and comparison photo Can energy, interval, media or upstream burr size be reduced?
Part-on-part marks or tangling Part orientation, load composition and affected surfaces Does the load need more separation, lower part quantity or different motion?
Media lodges in a feature Feature opening, media dimensions, frequency and removal method Which shape or size avoids the dimensional match?

E. Repeatability and release

  • Repeat trial ID and number of repeat batches: ____________________
  • Process window approved, conditional or rejected: ____________________
  • Variables that must not change without a new trial: ____________________
  • Inspection frequency for production: ____________________
  • Approved by / date / drawing or control-plan reference: ____________________

Methodology and related guides

The worksheet fields are derived from a basic controlled-trial principle: define acceptance first, document the starting condition, change limited variables, inspect representative features, and repeat the approved result before scale-up. For geometry-specific examples, see the guides for stamped metal parts and small fasteners. Equipment selection should follow the actual part, batch and acceptance criteria; the bowl, tub and capacity guide provides the broader decision framework.

The record-first principle can also be adapted to nonmetal workpieces, but the acceptance criteria must be rewritten for the material. Our separately operated jingseyewear site provides an example of a product category where surface appearance, edge condition and deformation risk require their own inspection language.

Version: 1.0, 20 July 2026. You may print or link to this worksheet for internal process planning. When sharing a completed record, remove customer-confidential drawings, part numbers, specifications and photographs unless disclosure is authorized.

#+86-592-2381506

Email : info@surface-polish.com

Headquarters address : No. 31, Xinchang Road, Xinyang Industrial Zone, Haicang District, Xiamen

click here to leave a message

Leave A Message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.

Home

Products

whatsapp

contact

สำหรับการสอบถามออนไลน์ โปรดใช้แบบฟอร์มติดต่อเรา